Cored Wire
Description:
Cored wire is manufacturing by crushing certain type of addictive (deoxidizer, desulfurizer, Modifier, alloy element) which added into liquid steel or molten iron to powder and then enveloped and closed with 0.35~0.45mm cold rolled steel strip into any length and lastly coiled and packed.
Typical usage:
Typical usage include ladle refining, tundish, steel & iron foundries, non-ferrous industries for inclusion modification, deoxidization, desulphurization, composition adjustment, microalloying, castability, prevention of clogging, inoculation.
Type and Size:
Taking into consideration the operation needs of steel and foundry industries, cored wire is not only available in common size cored wires but also can be produced as per customer’s special requests. |
|||||
Products |
Fill Rate (g/m) |
Chemical composition |
Applications |
||
Ø 9mm |
Ø 13mm |
Ø 16mm |
|||
CaSi |
120 |
225 |
330 |
Ca:30%min Si:55%min Al:1.5%max |
Suitable in desulphurization, deoxidation and modification of inclusions. |
CaFe |
140 |
260 |
360 |
Ca:30%min Fe:68%min Al:0.8%max |
For low Si steel, modifications of inclusions, desulphurization, deoxidation and avoids nozzle clogging when casting. |
C |
55 |
140 |
210 |
C:98.5%min Ash:0.45%max V:0.4%max |
Carbon fine adjustment, trimming addition. |
CaAIFe |
130 |
230 |
|
Ca:40% Fe:30% Al:30% |
Similar capabilities of CaFe with a further grain size improvement. |
FeTi |
170 |
365 |
570 |
Ti:65%-75%min Al:5%max Si:1%max |
For microalloying and deoxidation. |
FeB |
200 |
550 |
825 |
B:16%-18%min Al:0.5%max C:0.5%max |
For microalloying. |
MgFeSi |
90 |
210 |
330 |
Mg:23%-26%min Si:40%-45%min |
Used in modularization. |
Pure Al |
203 |
316 |
395 |
Al:99.7%min Si+Fe:0.3%max |
For deoxidation and grain size improvement. |
Pure S |
95 |
180 |
|
S:99%min |
Utilized in the resulphurising of engineering steels. |
FeSi |
150 |
350 |
|
Si:75%min Fe:Balance |
In nodularisation. |
Pure Ca |
58 |
155 |
- |
Ca:98.5%min Mg:0.5%max Al:0.5%max |
This PureCa in powder form for treatment low Si-Steel, modification of inclusions, avoid nozzle clogging when casting and improvement transverse mechanical properties of the steel. |
Solid Ca |
65 |
- |
- |
Ca:98.5%min Mg:0.5%max Al:0.5%max |
PureCa solid rod form, similar application as PuraCa in powder. High recovery rate during secondary metallurgical treatment of molten steel. |
Packing:
wrapped with plastic film, then mounted onto pallet, in vertical or horizontal way.
Diameter |
Coil Internal Diameter |
Coil External Diameter |
Coil Height & Width |
9mm土0.5mm |
600mm +/-10% |
1150mm +/-5% |
1100mm +/-10% |
13mm土0.5mm |
600mm +/-10% |
1150mm +/-5% |
1100mm +/-10% |
15mm土0.5mm |
600mm +/-10% |
1150mm +/-5% |
1100mm +/-10% |
16mm土0.5mm |
600mm +/-10% |
1150mm +/-5% |
1100mm +/-10% |
Feeding machine:
Feeding machine can be provided upon details: line root no, feeding speed, diameter, installation form (fixed/walking/rotating), motor type, operation place (LF/RH/Casting).